Intertek tests composite materials constituent content, using ASTM D Content analysis for composite materials ASTM D scope: The test method ASTM. Intertek tests composite materials constituent content, using ASTM D Content analysis for composite materials ASTM D scope: The test method. To extend the burn off test protocol in ASTM D to the determination of The current ASTM test method incorporates resin burn off as a way to determine.

Author: Gorn Goltilrajas
Country: Russian Federation
Language: English (Spanish)
Genre: Personal Growth
Published (Last): 17 May 2008
Pages: 499
PDF File Size: 5.79 Mb
ePub File Size: 6.46 Mb
ISBN: 824-4-50719-188-5
Downloads: 66903
Price: Free* [*Free Regsitration Required]
Uploader: Tami

Test Method II, applicable only to laminate materials of known fiber asfm weight, calculates reinforcement or matrix content by weight or volumeand the cured ply thickness, based on the measured thickness of the laminate.

Through our network of over 43, people in 1, laboratories and offices in countries, Intertek provides quality and safety solutions to a wide range of industries around the world.

The resulting solution is then filtered and the amount asgm remaining fiber is determined. Knowledge of the void volume of a composite material is desirable as an indication of d311 quality of a composite.

No other units of measurement are included in this standard. Testing Evaluating how your products and services meet and exceed quality, safety, sustainability and performance standards. Formally confirming that your products and services meet all trusted external and internal standards. The test is typically intended for two component materials. Procedures A through F are based on chemical removal of the matrix while Procedure G removes the matrix by igniting the matrix in a furnace. Link to Active This link will always route to the current Active version of the standard.

Enabling you to identify and mitigate the intrinsic risk in your operations, supply chains and business processes. The presence of voids is not measured. The suggested applications are discussed in Section 4, as well as at the start of each procedure. Work Item s – proposed revisions of this standard. See Section 9 for additional information. For method I, three specimens are machined from customer supplied product.

  ARDAS GURMUKHI PDF

Content Analysis for Composite Materials by ASTM D3171

A procedure for correction of the results for minor changes in the reinforcement is included. Astj, special provisions can be made to extend these test methods to filled material systems with more than two constituents, though not all test results can be determined in every case. Active view current version of standard. Referenced Documents purchase separately The documents listed below are referenced within the subject standard but are not provided as part of the standard.

Auditing Consulting Sourcing Training. Historical Version s – view previous versions of standard. Inspection Validating the specifications, value and safety of your raw materials, products ast, assets.

ASTM D – 11 Standard Test Methods for Constituent Content of Composite Materials

Also, knowledge of the constituent content is required for evaluation of the quality of a fabricated material and the processes used during fabrication. Test Method II, applicable only to laminate materials of d31171 fiber areal weight, calculates reinforcement or matrix content by weight or volumeand the cured ply thickness, based on the measured thickness of the laminate. Work Item s – proposed revisions of this standard.

The suggested applications are discussed in Section 4as well as at the start of each procedure. Method II is only for laminates and uses calculations based on thickness.

Evaluating astj your products and services meet and exceed quality, safety, sustainability and performance standards. The presence of voids is not measured. Whether your business is local or global, we can ensure your products meet quality, health, environmental, safety, and social accountability standards for virtually any market around the world. Eq d171 and 16 assume zero void content to perform the calculation.

Procedures A through F are based on chemical removal of the matrix while Procedure G removes the matrix by igniting the matrix in a furnace. Need help or have a question? Validating the specifications, value and asrm of your raw materials, products and assets.

See Section 9 for additional information. From the specimen density, constituent densities, and the fiber content, the reinforcement content, matrix content, and void content can then be determined.

  DIURESIS ACUOSA Y OSMOTICA PDF

Send us a request Need help or have a question?

Test Method II is not applicable to the measurement of dd3171 volume. No other units of measurement are included in this standard.

Higher void volumes usually mean lower fatigue resistance, greater susceptibility to moisture penetration and weathering, and increased variation or scatter in strength properties.

Send us a request Wilton UK: Global Reach Intertek is the industry leader with over 42, people in 1, locations in over countries. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

Method I removes the matrix by digestion or ignition. Assurance Testing Inspection Certification.

Referenced Documents purchase separately The documents listed below are referenced within the subject xstm but are not provided as part of the standard. However, special provisions can be made to extend these test methods to filled material systems with more than two constituents, though not all test results can be determined in every case.

A procedure for correction of the results for minor changes in the reinforcement is included.

Assurance Enabling you to identify and mitigate the intrinsic risk in your operations, supply chains and business processes.

Eq 9 and 10 assume zero void content to perform the calculation.

Link to Active This link will always route to the current Active version of the standard. The specimens are dried and cooled. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

The test method ASTM D provides two procedures for determining constituent content of composite materials.